Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrason® E 2010 NAT - PESU - BASF

Material Data Center offers the following functions for Ultrason® E 2010 NAT:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Ultrason E datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Unreinforced, medium viscosity standard injection moulding grade.
Abbreviated designation according to ISO 1043-1: PESU
Processing/Physical Characteristics乾燥/調湿単位テスト基準
ISO データ
メルトボリュームレイト, MVR 70 / * cm³/10min ISO 1133
温度 360 / * °C -
荷重 10 / * kg -
成形収縮率, 平行 0.8 / * % ISO 294-4, 2577
成形収縮率, 直角 0.9 / * % ISO 294-4, 2577
溶融時の密度 1230 kg/m³ -
溶融時の熱伝導率 0.18 W/(m K) -
溶融時の比熱 1950 J/(kg K) -
熱拡散率 7.53E-8 m²/s -
突き出し時の時の温度 200 °C -
ASTM数据
成形収縮率., 平行 0.007 mm/mm ASTM D 955
機械的特性乾燥/調湿単位テスト基準
ISO データ
引張弾性率 - / 2640 MPa ISO 527
降伏応力 - / 86 MPa ISO 527
降伏ひずみ - / 6.9 % ISO 527
引張クリープ弾性率, 1h * / 2800 MPa ISO 899-1
シャルピー衝撃強さ, +23°C - / N kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C - / N kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C - / 7.5 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C * / 8 kJ/m² ISO 179/1eA
ASTM数据
降伏応力 90.3 / - MPa ASTM D 638
降伏点伸び 6.7 / - % ASTM D 638
破断伸び 40 / - % ASTM D 638
曲げ弾性率 2599 / - MPa ASTM D 790
ノッチ付きIzod衝撃強さ, 1/8 in 10 / - J/m ASTM D 256
熱的特性乾燥/調湿単位テスト基準
ISO データ
ガラス転移点, 10°C/min 225 / * °C ISO 11357-1/-2
荷重たわみ温度, 1.80 MPa 205 / * °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 218 / * °C ISO 75-1/-2
ビカット軟化温度, B 215 / * °C ISO 306
線膨張係数, 平行 52 / * E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 V-0 / * class IEC 60695-11-10
試験片の厚さ 1.6 / * mm -
Yellow Card 可用 はい / * - -
厚さhでの燃焼性 V-0 / * class IEC 60695-11-10
試験片の厚さ 3.0 / * mm -
Yellow Card 可用 はい / * - -
厚さhでの燃焼性 5V 5VA / * class IEC 60695-11-20
試験片の厚さ 3.0 / * mm -
Yellow Card 可用 はい / * - -
酸素指数 38 / * % ISO 4589-1/-2
ASTM数据
線膨張係数, 直角 59.9 E-6/K ASTM D 696
DTUL @ 66 psi 208 °C ASTM D 648
DTUL @ 264 psi 195 °C ASTM D 648
電気的特性.乾燥/調湿単位テスト基準
ISO データ
比誘電率, 100Hz * / 3.9 - IEC 62631-2-1
比誘電率, 1MHz * / 3.8 - IEC 62631-2-1
誘電正接, 100Hz * / 17 E-4 IEC 62631-2-1
誘電正接, 1MHz * / 140 E-4 IEC 62631-2-1
体積抵抗率 * / >1E13 Ohm*m IEC 62631-3-1
表面抵抗率 * / >1E15 Ohm IEC 62631-3-2
耐電圧 * / 37 kV/mm IEC 60243-1
耐トラッキング性 * / 125 - IEC 60112
その他の特性.乾燥/調湿単位テスト基準
吸水率 2.2 / * % Sim. to ISO 62
吸湿率 0.8 / * % Sim. to ISO 62
密度 1370 / - kg/m³ ISO 1183
密度 1370 kg/m³ ASTM D 792
材料特有の特性乾燥/調湿単位テスト基準
ISO データ
粘度数 56 / * cm³/g ISO 307, 1157, 1628
試験片の成形条件.単位テスト基準
ISO データ
射出成形, 樹脂温度 360 °C ISO 294
射出成形, 金型温度 160 °C ISO 294
射出成形, 射出速度 200 mm/s ISO 294
射出成形, 保圧 70 MPa ISO 294
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 140 °C -
Pre-drying - Time 4 h -
Processing humidity ≤0.02 % -
樹脂温度 340 - 390 °C -
金型温度 140 - 180 °C -
機能
 粘度せん断速度. , Ultrason® E 2010 NAT, PESU, BASF
 せん断応力-せん断速度. , Ultrason® E 2010 NAT, PESU, BASF
 せん断弾性率-温度. , Ultrason® E 2010 NAT (乾燥), PESU, BASF
 応力-ひずみ. , Ultrason® E 2010 NAT (調湿), PESU, BASF
 割線弾性率−ひずみ. , Ultrason® E 2010 NAT (調湿), PESU, BASF
 pvT , Ultrason® E 2010 NAT, PESU, BASF
 引張弾性率-温度. , Ultrason® E 2010 NAT (調湿), PESU, BASF
Fatigue strength , Ultrason® E 2010 NAT, PESU, BASF
特殊な特性
成形加工法.
射出成形., フィルム押出成形., 異形押出成形., シート押出成形., ブロー成形., 熱成形.
納入形状.
ペレット., ナチュラルカラー
領域別の利用可能性
その他の情報
村遜速揃
PREPROCESSING
Pre/Post-processing, max. allowed water content: .02 %
Pre/Post-processing, Pre-drying, Temperature: 140 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 340 - 390 °C
injection molding, Melt temperature, recommended: 360 °C
injection molding, Mold temperature, range: 140 - 180 °C
injection molding, Mold temperature, recommended: 160 °C
injection molding, Dwell time, thermoplastics: 10 min

Pretreatment
Drying temperature: 130 - 150°C
Drying time: minimum 4h
recommended dryer: vaccum or dry air dryer
maximum moisture: 0,02 - 0,05%

Ultrason® can be injection molded by any type of machinery on the market, provided that the plasticizing unit and the mold temperature control system have been configured appropriately. The machinery manufacturer must be consulted if any doubts exist on the ability of various parts to withstand the high temperatures required (e.g. barrel, barrel head, bolted connections, etc.)

Long residence time in combination with high temperatures should be avoided e.g. by pump out material at regular intervals.
During extended interruptions, the barrel temperature should be lowered to about 250-280°C.

It has been found out that heating to the requested processing temperature and shutting down or lowering the temperature is best carried out in two steps.
First, the barrel temperatures are set at the lower processing temperature range for the particular thermoplastic (340 - 350 °C). As soon as these temperatures have reached a steady state, the material in the barrel is pumped out. Second, the barrel temperature can be set to the required processing temperature or the heaters can be shut down.
耐薬品性
5wt%酢酸 (23゚C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com